ASC BRICK FOR IRON LADLE
WHO WE ARE :
We not only provide the best service to World Top 500 Enterprises , also to YOU .
We can accept the Payment Term : LC 120 DAYS , D/P 90 DAYS, D/A-O/A 60 DAYS .
We have more 100 items Chinese National Patents .
Our Lab is Hennan province Refractory Engineering T&R Center
Our Tech Team include : PROFESSOR , DOCTORAL SUPERVISOR , SENIOR ENGINEER, EXPERT.
Our Project Team have rich experience for international Refractory Turn-Key Project .
We are not only to supply refractory products to YOU , We also want to share the KEY TECH with YOU.
ASC BRICK & CASTABLE FOR THE IRON LADLE
LIFE > 1200 HEATS .
It is mainly raw material made of electro-corundum (or sintered corundum, special glass bauxite clinker) and graphite and silicon carbide containing more than 90%-95% of fixed carbon.Add graphite, bauxite and additives, and make them by mixing, moulding, drying and firing at high temperature.
1、铝碳化硅碳砖 – ASC BRICK
项 目 ITEM |
单位 |
指标值 |
体积密度 BD |
g/cm3 |
≥2.85 |
常温耐压强度 CCS |
Mpa |
≥40 |
高温抗折强度(1400℃×0.5h)MOR |
Mpa |
≥5 |
Al2O3 |
% |
55-65 |
C |
% |
5-12 |
SiC |
% |
8-10 |
2、铝碳化硅浇注料 – ASC CASTABLE (REPAIR CASTABLE )
项 目 ITEM |
单位 |
指标值 |
|
Al2O3 |
% |
55-65 |
|
SiC |
% |
6-10 |
|
耐火度 REFRACTORINESS |
℃ |
>1790 |
|
体积密度 BD |
g/cm3 |
≥2.6 |
|
抗折强度 MOR |
110℃×24h |
Mpa |
≥6 |
1500℃×3h |
Mpa |
≥10 |
|
耐压强度 CCS |
110℃×24h |
Mpa |
≥50 |
1500℃×3h |
Mpa |
≥80 |
|
烧后线变化 PLC |
1500℃×3h |
% |
±1 |